Non-Ohmics and Electrical properties of CaCu3Ti4O12 doped strontium ceramics prepared by a polymer pyrolysis method
View/ Open
Date
2014Author
Sunun Nonglek
Jakkawal Chaiyaput
Thanin Putjuso
Metadata
Show full item recordAbstract
This research is prepared the CSrCT0.35O-0, CSrCT0.35O-3, CSrCT0.35O-10 and
CSrCT0.35O-20 powders by using the polymerpyrolysis solution method. Microstructure
and phase composition were characterized by scanning electron microscopy (SEM) and
X-ray diffraction (XRD). Study the electrical properties as at room temperature and 1
kHz. Study the influences of non-linear current voltage
The results showed that the particles in the range of 2-5 micrometer of the
prepared powder at calcined temperatures at 850 ºC for 9h. XRD result displays the
main peaks of CCTO and small amount of TiO2 and CuO for all powders and ceramics
samples. The SEM study showed small and large grain sizes and the EDX displays
amount of doped strontium at small grain size higher than large grain size. At room
temperature and 1 kHz the ceramic sample doped amount 0.10 %wt showed large
dielectric constants ( 95904) while the ceramic sample doped 0.20 %wt showed
small dielectric loss tangents (tan0.074). In additionally, the ceramic sample doped
Sr with x=0.20 showed high non-linear coefficient () and breakdown field (Eb) values
of 5.6 and 1859, respectively