dc.description.abstractThe hole flange ability can be evaluated by limiting hole expansion ratio from hole expansion test. High strength steel grade 590 and 780 with 1.2 mm of thickness were used in this research. This results showed that the hole cut by laser and pierced by piercing punch which cause changing in microstructure thus increasing hardness introduced low ability of hole flanging. From experimental results, it was found that the hole making by wire cut process shows highest hole expansion ratio. The hole from piercing with counter punch can be increased the hole expansion ratio more than hole from piercing process.en_US
dc.language.isoTHen_US
dc.publisherRajamangala University Of Technology Rattanakosinen_US
dc.subjectHigh strength steelen_US
dc.subjectHole expansion ratioen_US
dc.subjectPiercing processen_US
dc.titleInfluence of Micro Crack to Hole expansion behavior of High Strength Steel Sheeten_US
dc.title.alternativeอิทธิพลของรอยแตกในระดับจุลภาคที่ส่งผลต่อพฤติกรรมการขยายตัวของเหล็กกล้าความแข็งแรงสูงen_US
dc.typeResearchen_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record